1. Grade Overview
16MnCr5 is a case hardening steel defined in EN 10084, used for components that need a hard wear resistant surface and a tough core. The name indicates a nominal carbon content of 0.16 percent with manganese and chromium as the main alloying elements. The steel is supplied as hot rolled round bar, forged round bar and in smaller sizes as peeled or ground bar, and the normal delivery condition is annealed so that the material can be machined easily before hardening.
2. Chemical Composition
The composition of 16MnCr5 is controlled to give consistent hardenability and a clean case after carburizing. A typical range is carbon 0.14 to 0.19 percent, silicon 0.40 percent maximum, manganese 1.00 to 1.30 percent, chromium 0.80 to 1.10 percent, phosphorus 0.025 percent maximum and sulphur 0.035 percent maximum. Chromium is the main hardenability element, and the fine control of manganese keeps the case hardness uniform around the bar circumference.
| Element | Typical Range in Percent |
| Carbon | 0.14 - 0.19 |
| Silicon | 0.40 max |
| Manganese | 1.00 - 1.30 |
| Chromium | 0.80 - 1.10 |
| Phosphorus | 0.025 max |
| Sulphur | 0.035 max |
3. Heat Treatment Process
Case hardening starts with carburizing at 880 to 980°C in a carbon rich atmosphere, which raises the carbon content of the surface layer to about 0.8 percent. The part is then quenched directly or after re-heating to 820 to 850°C, followed by tempering at 150 to 200°C. The result is a hard martensitic case with a hardness of 58 to 62 HRC and a tough, low carbon core. For forgings, a normalizing treatment before machining refines the grain and prepares the structure for carburizing.
4. Mechanical Properties of the Bar
In the hardened and tempered condition the core develops a tensile strength in the range of roughly 880 to 1180 MPa depending on the bar diameter, with good ductility and impact toughness. The case hardness and the case depth are controlled by the carburizing cycle and are verified by hardness traverse tests on a sample from each batch. The combination of a hard case and a tough core gives gear teeth and shafts excellent resistance to wear, pitting and bending fatigue.
5. Typical Applications
Gears, pinions and gear shafts in transmissions.
Camshafts, rocker arms and valve train components.
Piston pins, universal joint crosses and bearing races.
Bushings, rollers and sliding blocks.
Forged blanks for heavy vehicle and machine components.
Frequently Asked Questions
Q: What does 16MnCr5 mean in the EN 10084 system? The 16 indicates a nominal carbon content of 0.16 percent, Mn shows a manganese alloying addition of about 1 percent and Cr shows a chromium addition of about 1 percent.
Q: Why is 16MnCr5 called a case hardening steel? It is designed to be carburized and hardened so that only the surface layer becomes hard and wear resistant, while the core stays tough and ductile to resist impact loads.
Q: What is the delivery condition of the round bar? The bar is normally supplied in the annealed condition for machining, and it can also be supplied normalized, peeled, turned or ground to a close diameter tolerance.
Q: What hardness can be reached on the case? A properly carburized and quenched case reaches about 58 to 62 HRC, and the case depth is specified on the drawing and verified by hardness traverse testing.
Q: Can 16MnCr5 be induction hardened instead? Yes, induction hardening can be applied to selected areas, but for uniform full case hardness on complex shapes carburizing is the standard and more reliable process.