Products Description
S355J2W meaning: S is structural steel, 355 is the yield strength of 355MPa, J2 requires -20° impact, the letter W indicates that the steel has the ability to resist atmospheric corrosion.

S355J2WP meaning: S355J2WP is high phosphorus corrosion resistant structural steel. S is structural steel, 355 is the yield strength of 355MPa, J2 requires -20° impact, the letter W indicates that the steel has the ability to resist atmospheric corrosion, and P is the chemical element phosphorus.
Chemical Composition
| Grade | C max | Si max |
Mn max |
P max | S max | N max |
Cr max | Cu max |
| S355J2W | 0.16 | 0.50 | 0.50-1.50 | 0.030 | 0.035 | – | 0.40-0.80 | 0.25-0.55 |
| Grade | C | Si | Mn | P | S | Cu | Cr | CEV |
|---|---|---|---|---|---|---|---|---|
| – | maximum % |
maximum % |
maximum % |
% | maximum % |
% | % | maximum % |
| S355J2WP corten steel plate | 0,12 | 0,75 | 1,0 | 0,06 – 0,15 | 0,030 | 0,25 – 0,55 | 0,30 – 1,25 | 0,52 |
Mechanical & Physical Properties
| Grade | Min Yield strength in different thickness | Min tensile strength in different thickness | Elongation in different thickness | ||||||||||||||
| S355J2W | ≤ 16 |
> 16 ≤ 40 |
> 40 ≤ 63 |
> 63 ≤ 80 |
> 80 ≤ 100 |
> 100 ≤ 150 |
≤ 3 |
> 3 ≤ 100 |
> 100 ≤ 150 | ≤ 1.5 | > 2 ≤ 2.5 | > 2.5 ≤ 3 | > 3 ≤ 40 |
> 40 ≤ 63 |
> 63 ≤ 100 |
> 100 ≤ 150 | |
| 355 | 345 | 335 | 325 | 315 | 295 | 510- 680 |
470- 630 |
450-600 | 16 | 17 | 18 | 22 | 21 | 20 | 18 | ||
| Grade | Tensile strength Rm | Yield strength Reh | Elongation – A | Minimum elongation – A | ||||
| – | MPa | (Minimum) MPa |
Lo = 80 mm (minimum) | Lo = 5,65 * √So (%) | ||||
| – | Thickness mm |
Thickness mm |
Thickness mm |
– | ||||
| – | ≤3 | >3 ≤100 |
≤16 | >16 ≤40 |
>1,5 ≤2 |
>2 ≤2,5 |
>2,5 ≤3 |
>3 ≤40 |
| S355J2WP corten steel plate | 510-680 | 470-630 | 355 | 345 | 16 | 17 | 18 | 22 |
The difference of S255J2W and S355J2WP
First of all, S355J2WP and S355J2W are structural steels under the European standard EN 10025-5. They are specially designed to improve resistance to atmospheric corrosion and are commonly used in outdoor structures and buildings exposed to harsh weather conditions.
The main difference between these two grades lies in their chemical composition. S355J2WP contains a higher amount of phosphorus and a lower amount of copper compared with S355J2W. The additional phosphorus forms a protective layer on the surface, thereby enhancing the steel's atmospheric corrosion resistance. Meanwhile, the lower copper content makes S355J2WP more resistant to corrosion in chloride-containing environments.
In terms of mechanical properties, the two grades are quite similar. Both have a minimum yield strength of 355 N/mm² and are widely applied in construction and engineering fields. However, S355J2WP offers higher impact toughness and slightly higher tensile strength compared with S355J2W.
Another important difference is their applicable temperature range. S355J2WP is suitable for environments up to 500°C, while S355J2W can be used at temperatures up to 600°C. This variation in temperature resistance makes each grade suitable for different working conditions and applications.
Regarding surface appearance, S355J2W is often favored for its aesthetic appeal. It has a smooth and uniform finish, making it a popular choice for architectural facades and cladding. Due to the presence of phosphorus, however, S355J2WP may have a relatively rougher surface, which in some cases may affect the desired aesthetics.
In terms of availability and cost, both grades are widely available in the market. However, because of the additional phosphorus content, S355J2WP is generally more expensive than S355J2W. This cost difference becomes an important factor to consider, especially for large-scale projects.