Multi-Grade Hot Rolled Steel Angle Supply
Structural angle sections are ordered by shape and by material grade, and international projects frequently mix several grade systems on the same drawing set. A supply covering ASTM A36, EN 10025-2 S275 and S355, JIS G 3101 SS400, ASTM A131 marine grade AH36 and GB/T 700 Q195 lets a fabricator keep one section family while matching the material to each part of the structure: general frames in A36 or S275, heavily loaded members in S355, light secondary steel in Q195, and hull or deck details in AH36. All of these angles are produced by the same hot rolling route, passing billets through grooved rolls at 900–1100 °C, which refines the grain structure, improves toughness and produces a clean surface that accepts galvanizing and paint systems readily.
Grade-by-Grade Property Reference
The table below gives the specified minimum properties that matter for design and inspection. Values are quoted for thickness up to 16 mm, which covers the majority of angle sizes.
| Grade | Standard | Minimum yield strength | Tensile strength | Notes |
|---|---|---|---|---|
| A36 | ASTM A36/A36M | 250 MPa (36 ksi) | 400–550 MPa | General structural framing, excellent weldability |
| S275 | EN 10025-2 | 275 MPa | 410–560 MPa | Medium-duty frames and bracing |
| S355 | EN 10025-2 | 355 MPa | 470–630 MPa | Heavy structural and bridge components |
| SS400 | JIS G 3101 | 245 MPa | 400–510 MPa | General construction and equipment frames |
| AH36 | ASTM A131/A131M and ABS rules | 355 MPa | 490–620 MPa | Hull, deck and offshore details, impact tested at 0 °C |
| Q195 | GB/T 700-2006 | 195 MPa | 315–430 MPa | Light-duty racks, guards and partitions |
The designation systems are not interchangeable even where strengths coincide. ASTM A6/A6M is often quoted on the same line as A36, and it is worth being precise about what it contains: A6/A6M is a specification of general requirements for rolled structural steel bars, plates, shapes and sheet piling, covering ordering practice, dimensional tolerances, permissible variations in mass and length, and the test methods used to verify a grade. It does not itself define a strength grade, so an angle cannot be ordered "to A6" alone; A36/A36M supplies the mechanical and chemical requirements and A6/A6M supplies the tolerance framework around them. Similarly, AH36 belongs to the higher-strength marine family governed by ASTM A131/A131M and by classification society rules, with an impact test at 0 °C that standard structural grades do not require.
Specifications 100 × 100 × 6 and 160 × 160 × 10
Two sizes are requested most often for general fabrication because they bracket the range between medium bracing and heavier frame work. Both are equal-legged, so the section behaves uniformly about both principal axes.
| Size (mm) | Mass by table (kg/m) | Mass by nominal formula (kg/m) | Typical use |
|---|---|---|---|
| 100 × 100 × 6 | 9.22 | 9.14 | Truss chords, purlins, beam connections, stair strings |
| 160 × 160 × 10 | approx. 24.6 | 24.34 | Column bracing, machine bases, heavy frames |
The nominal mass per metre follows W = t × (2e − t) × 0.00785, where e is leg length in millimetres, t is thickness in millimetres and 7.85 g/cm³ is the density of steel. Table values are marginally higher because the rounded corner radius adds area; the difference is under one per cent and does not affect structural calculations, but it should be understood when reconciling order weights with a shipment. Leg length, thickness, squareness, straightness and camber all fall under the dimensional tolerances of the relevant product standard, and inspection records should state measured values rather than nominal ones.
Fabrication and Welding Across the Grade Range
Cutting, punching and drilling practice is essentially identical for the whole family, since all six grades are ferritic carbon or low-alloy steels with similar hardness in the as-rolled condition. Welding is where the grades diverge. A36, S275, SS400 and Q195 have low carbon equivalents and can be welded with standard electrodes without preheat for sections under 20–25 mm in mild weather. S355 and AH36 carry higher strength through micro-alloying and slightly higher carbon, so thicker sections, restrained joints and cold ambient conditions call for preheat in the 80–150 °C range, low-hydrogen consumables, and control of heat input to avoid grain coarsening in the heat-affected zone. AH36 is a toughness-critical marine grade, so its welding procedure should be qualified with impact testing of the joint rather than relying on parent metal data alone. In every case, thermal cut edges should be ground clean before a full-penetration weld is made, and heat input records should accompany the procedure qualification.
Marine Service and Coating Selection for AH36
Angles used in hull, deck, hatch and offshore details require more than a standard paint system. The usual specification is blast cleaning followed by a zinc-rich primer and a high-build epoxy system, often with a polyurethane topcoat for colour and gloss retention, and the total dry film thickness is verified coat by coat. Where angles are galvanized instead, ISO 1461 or ASTM A123/A123M coatings of typically 70–85 µm on thick sections provide barrier and sacrificial protection, and cut ends or weld areas must be repaired with a zinc-rich coating to restore continuity. AH36 sections intended for hulls may also be supplied with classification society certification and impact test records at 0 °C, so the mill test documentation should be checked against the project's survey requirements before fabrication starts.
Frequently Asked Questions
Q: What grades of hot rolled steel angle are available in one section family?
Angles can be rolled in ASTM A36, EN 10025-2 S275 and S355, JIS G 3101 SS400, ASTM A131/A131M AH36 and GB/T 700-2006 Q195, covering minimum yield strengths from 195 MPa to 355 MPa. The same leg sizes and lengths are available across the range, so one section family can serve several parts of a project.
Q: What is ASTM A6/A6M, and does it define a steel grade?
A6/A6M is a general requirements specification for rolled structural steel bars, plates, shapes and sheet piling. It covers ordering practice, dimensional tolerances, mass and length variations and test methods, but it does not set yield or tensile strength. The grade must be called up separately, as in A36/A36M, with A6/A6M supplying the tolerance framework.
Q: How do A36, S275, S355 and SS400 compare in strength?
Minimum yield strengths are 250 MPa for A36, 275 MPa for S275, 355 MPa for S355 and 245 MPa for SS400, with tensile ranges of 400–550 MPa, 410–560 MPa, 470–630 MPa and 400–510 MPa respectively. A36, S275 and SS400 behave similarly in general framing, while S355 is chosen for heavy or highly stressed members.
Q: What is AH36 angle used for?
AH36 is a higher-strength marine grade supplied to ASTM A131/A131M and classification society rules, with a 355 MPa minimum yield strength, a 490–620 MPa tensile range and impact testing at 0 °C. It is used for hull stiffeners, deck structures, hatch coamings, offshore platforms and other details exposed to wave loading and low temperatures.
Q: Where does Q195 angle fit in light-duty structures?
Q195 to GB/T 700-2006 has a 195 MPa minimum yield strength and a 315–430 MPa tensile range, which suits storage racks, guards, partition framing, cable trays and similar non-critical members. It is not appropriate for primary load-bearing frames, where A36, S275 or S355 should be specified.
Q: How is the mass of a steel angle calculated?
Use W = t × (2e − t) × 0.00785 with leg length e and thickness t in millimetres, based on a steel density of 7.85 g/cm³. A 100 × 100 × 6 mm angle gives about 9.14 kg/m by formula and 9.22 kg/m from standard tables, the small difference coming from the rounded corner radius.