How do the mechanical properties of GB Q355B and ASTM A572 Grade 50 angles compare?

Nov 26, 2025

Leave a message

The mechanical properties of Q355B and A572 Grade 50 are highly comparable, forming the basis for their equivalence. Both specify a minimum yield strength of 345 MPa (50 ksi) and a minimum tensile strength in the range of 450-630 MPa for Q355B and 65 ksi (450 MPa) for A572 Gr.50. The minimum elongation is also similar, typically around 21% for a standard gauge length, indicating good ductility. The key mechanical difference often lies in the testing and certification of impact toughness. Q355B, as a Grade B quality, requires a minimum Charpy V-notch impact energy of 34J at 20°C. For A572 Gr.50, impact testing is not a mandatory requirement unless specified by the purchaser, in which case it is tested per ASTM A673 with frequencies and temperatures agreed upon. Therefore, when substituting, it is crucial to confirm that the Q355B material meets any required impact toughness at the service temperature, as its standard requirement is only for room temperature.