How does the chemical composition of 316Ti stainless round steel differ from 316L, and what chemical role does titanium play in high-temperature service?​

Sep 17, 2025

Leave a message

 

316Ti stainless round steel (ASTM A276; GB 06Cr17Ni12Mo2Ti) has a composition of 16.0–18.0% chromium (Cr), 10.0–14.0% nickel (Ni), 2.0–3.0% molybdenum (Mo), 0.04–0.10% titanium (Ti), ≤0.08% carbon (C), ≤1.00% silicon (Si), ≤2.00% manganese (Mn), ≤0.045% P, ≤0.030% S.​

Compared to 316L (no intentional Ti), 316Ti's titanium (0.04–0.10%) plays a critical role in high-temperature service by preventing carbide-induced degradation: At temperatures above 500°C, carbon in 316L reacts with chromium to form Cr₂₃C₆ carbides at grain boundaries, depleting chromium near boundaries and breaking down the passive Cr₂O₃ layer (intergranular corrosion). Titanium in 316Ti has a higher affinity for carbon than chromium-it reacts with carbon to form stable TiC carbides in the matrix, not at grain boundaries. This "traps" carbon, preventing it from migrating to boundaries and depleting chromium.​

At high temperatures, TiC also resists coarsening better than Cr₂₃C₆, maintaining its ability to pin dislocations and strengthen the steel. This makes 316Ti suitable for service at 500–650°C, whereas 316L degrades above 450°C due to intergranular corrosion. Molybdenum and nickel function the same as in 316L, providing chloride resistance and austenite stabilization.