How the NM Series Is Structured
The NM designation combines the letters for wear resistance with a number that represents the nominal Brinell hardness of the plate surface. NM400, NM500 and NM600 therefore target nominal values of 400, 500 and 600 HBW. The grade system and the permitted hardness range around each nominal value are defined in GB/T 24186, and hardness is verified by the Brinell method described in GB/T 231.1, with ISO 6506-1 used as the equivalent international procedure.
All NM grades are delivered in the quenched and tempered condition. The low-alloy composition, typically built around carbon, manganese, silicon, chromium, and often boron or molybdenum additions, is designed so that the plate hardens through a controlled quench and then tempers to a tough, wear-resistant microstructure rather than a brittle one.
Hardness, Microstructure and Wear Life
Hardness is the property that most directly controls resistance to sliding and impact abrasion. Raising the nominal hardness from 400 to 500 HBW increases resistance to low-stress scratching abrasion substantially, because the abrasive particles in ore, coal, sand and aggregate are less able to indent and cut the surface. The relationship is not linear with hardness alone, since microstructure, inclusion content and toughness also govern how the plate behaves under gouging or high-impact conditions.
| Grade | Nominal surface hardness | Typical use |
|---|---|---|
| NM400 | 400 HBW | General chute, hopper and bucket liners |
| NM500 | 500 HBW | High-abrasion liners, crusher and transfer points |
| NM600 | 600 HBW | Severe sliding abrasion with limited impact |
Comparative abrasion testing is carried out with the dry sand rubber wheel method of ASTM G65, which reports volume loss under a controlled abrasive flow. Where two candidate grades are close in hardness, that test gives a more useful comparison than hardness figures alone.
Thickness Range and Practical Availability
Wear plate is commonly supplied from about 3 mm up to 100 mm. Thin plate in the 3 to 8 mm range is used for chute liners and truck bed sections where weight matters. Plate from 20 mm to 60 mm is used for crusher linings, hopper bottoms and impact zones. As thickness increases, the depth to which the specified hardness is guaranteed becomes a purchasing question: hardness is normally measured near the surface, and the core may be softer, so the order should define whether the requirement applies to the surface, to a stated depth below the surface, or to the mid-thickness.
Higher nominal hardness also narrows the practical thickness window. NM600 is generally offered in a more limited thickness range than NM400, because achieving 600 HBW through a heavy section requires a higher alloy content and a more severe quench, both of which increase cracking risk during processing.
Cutting, Forming and Machining
Wear plate can be cut by plasma, laser, waterjet or oxy-fuel. Oxy-fuel and plasma cutting leave a heat-affected zone at the cut edge with hardness different from the parent plate; the edge should be ground back before bending, and small radius bends close to a cut edge should be avoided. Drilling requires carbide tooling at low speed and positive feed, since the plate is too hard for high-speed steel tooling. Cold forming is limited: minimum bend radii are generous, and forming should be done transverse to the rolling direction where possible.
Welding Practice for Abrasion-Resistant Plate
Welding a quenched and tempered wear plate alters the heat-affected zone, creating a soft band on the parent-metal side and a hard, crack-susceptible zone in the weld itself. Standard practice is to use low-hydrogen consumables, apply preheat in the range required for the plate thickness and carbon equivalent, control heat input, and where the joint will experience wear, overlay the weld with a hardfacing deposit or protect it with a bolted liner. Wherever the design permits, bolting or mechanical fastening avoids the problem entirely.
Ordering Checklist
State the standard and grade, nominal hardness, minimum hardness at the required depth, delivery condition, thickness and thickness tolerance, flatness limit, edge condition, and whether ultrasonic examination is required. Request a certificate reporting the hardness test position and the number of tests, and confirm the plate marking before releasing the material to fabrication.
Frequently Asked Questions
Q: What does the number in NM500 indicate?
A: It indicates the nominal Brinell hardness of the plate surface, 500 HBW, with the grade and its hardness range defined in GB/T 24186.
Q: Which grade should be used for a crusher liner with impact loading?
A: A toughness-preserving grade such as NM400 or NM450 is usually better than NM600, because very high hardness grades trade impact toughness for wear resistance.
Q: How is wear plate hardness tested?
A: By the Brinell method under GB/T 231.1 or the equivalent ISO 6506-1 procedure, normally on a prepared surface at a defined depth below the rolled surface.
Q: Can NM500 plate be bent?
A: Only with generous bend radii and after the cut edge has been dressed. Cold forming limits are much tighter than for structural carbon steel of the same thickness.
Q: Is the hardness the same through the whole thickness?
A: No. Full hardness is normally specified near the surface, and core hardness is lower on thick plate, so the purchasing specification must state the depth at which hardness applies.
Q: What consumable should be used when welding wear plate?
A: A low-hydrogen consumable matched to the base metal strength, applied with preheat and controlled heat input, followed by hardfacing where the welded area will be exposed to abrasion.