Equal Angle Steel in ASTM A36, Q235 and Q355 Grades

Jan 12, 2026

Leave a message

What an Equal Angle Section Is

An equal angle is a rolled steel section with two legs of the same width meeting at 90 degrees, forming an L-shaped profile. The shape resists bending and torsion efficiently and provides flat faces for bolting and welding, which makes it one of the most used sections in steel construction.

Grade Options and Properties

ASTM A36: minimum yield 250 MPa, tensile 400-550 MPa, the default grade for US-based designs

Q235 (GB/T 700-2006): minimum yield 235 MPa, tensile 370-500 MPa, with B, C and D impact classes

Q355 (GB/T 1591-2018): minimum yield 355 MPa, tensile 470-630 MPa, for higher-strength designs; Q355 is the successor to Q345

For rolled angle sections the applicable ASTM standard is A36; ASTM A53 covers welded steel pipe and is not applied to angle profiles.

Size Range and Dimensions

Equal angles are rolled from 20 x 20 x 3 mm up to 200 x 200 x 24 mm in the GB/T 706-2016 series, with imperial sizes available for US projects. The size is described as leg width x leg width x thickness, for example L50x50x5, and standard lengths are 6 m and 12 m.

Tolerances and Surface

Leg width, thickness, length and straightness are controlled to the governing standard, GB/T 706-2016 or ASTM A6/A6M. The surface of hot-rolled angle is free of harmful defects, with the normal mill scale present. Surfaces can be delivered black, oiled, primed or hot-dip galvanized to BS EN ISO 1461.

Selection Guidance

Choose the grade that matches the design code of the project. For general framing, Q235 and A36 are economical; where spans are long or loads are high, Q355 reduces the section size needed. The impact class should be selected for the service temperature of the structure.

Typical Applications

Trusses, lattice towers and bracing

Frames for buildings, platforms and equipment

Brackets, cleats and connection details

Shelving, racks and cable supports

Fences, gates and agricultural structures

Frequently Asked Questions

Q: Is Q235 equivalent to ASTM A36?
They are similar carbon structural steels and are often interchanged for secondary structures, but A36 guarantees 250 MPa yield against 235 MPa for Q235, so check the design stress.

Q: Is Q345 still available?
Q345 was replaced by Q355 in GB/T 1591-2018. New specifications should call for Q355, which has the same nominal yield of 355 MPa.

Q: What does L50x50x5 mean?
It describes an equal angle with 50 mm legs and 5 mm thickness, the standard way of identifying angle sections.

Q: Can equal angles be galvanized?
Yes, hot-dip galvanizing to BS EN ISO 1461 is standard for outdoor angle steel, protecting the sections for decades.

Q: What lengths are supplied?
Standard lengths are 6 m and 12 m, with cutting to exact length and punching or drilling available before despatch.

Q: Which grade is used for transmission towers?
Tower legs and bracing commonly use Q355 or equivalent high-strength grades to keep the structure light, with Q235 used for secondary members.