S355 Round Bars and the Legacy S355J2G3 Name
S355 round bar is a hot rolled or peeled circular long product supplied in the structural steel grades defined by EN 10025-2. Drawings that date from the older EN 10025 edition often carry the designation S355J2G3; that name has been withdrawn and the equivalent current designation is S355J2, with the same minimum yield strength of 355 MPa and the same guaranteed impact energy at −20 °C. Similarly, the old S355JR and S355J0 names used for the same family remain valid in the current standard, so a buyer converting an old specification only has to map S355J2G3 to S355J2 rather than change the strength requirement.
S355 Is a Non-Alloy Structural Steel
A common misconception is that the 355 in the designation indicates an alloy steel. It does not. S355JR and S355J2 are classified as non-alloy structural steels in EN 10025-2, and their strength comes from a manganese content of up to 1.60 percent combined with controlled rolling or normalising rather than from deliberate additions of chromium, nickel or molybdenum. Genuine alloy steel bars, such as quenched and tempered chromium-molybdenum grades used for stressed shafts, gears and tools, are covered by separate standards and carry much higher alloy content. The practical consequence is that S355 bars weld and machine like a structural steel, not like a heat treated alloy bar.
Mechanical Properties and Impact Grades
| Designation | Minimum yield strength | Tensile strength | Elongation | Impact energy |
|---|---|---|---|---|
| S355JR | 355 MPa | 470–630 MPa | ≥ 22 % | 27 J at +20 °C |
| S355J0 | 355 MPa | 470–630 MPa | ≥ 22 % | 27 J at 0 °C |
| S355J2 | 355 MPa | 470–630 MPa | ≥ 22 % | 27 J at −20 °C |
| S355K2 | 355 MPa | 470–630 MPa | ≥ 22 % | 40 J at −20 °C |
The values apply to the normal thickness range up to 16 mm, with the yield strength figure reducing in steps as thickness increases, so the thickness dependent table in the standard governs the acceptance of a test piece. All four designations share the same strength level and differ only in the toughness they guarantee, which makes the impact grade the decisive choice for outdoor, cold climate or dynamically loaded components.
Chemistry and Carbon Equivalent
| Element | S355JR limit | S355J2 limit |
|---|---|---|
| Carbon | 0.22 % max | 0.20 % max |
| Silicon | 0.55 % max | 0.55 % max |
| Manganese | 1.60 % max | 1.60 % max |
| Phosphorus | 0.035 % max | 0.030 % max |
| Sulphur | 0.035 % max | 0.030 % max |
| Carbon equivalent | 0.45 max | 0.45 max |
The tighter phosphorus and sulphur limits are part of what the J2 grade buys in addition to the lower impact temperature. The carbon equivalent value of 0.45 applies to the thickness range stated in the standard and is the parameter that welding procedures are built around, because it governs hardenability in the heat affected zone and therefore the risk of cold cracking.
Size Range, Tolerance and Finish
Hot rolled bars: 16 mm to 320 mm diameter, with forged bars available above that range.
Cold drawn bars: 3 mm to 100 mm, work hardened in the drawing operation, so the mechanical values differ from the hot rolled tables.
Peeled and polished bars: 20 mm to 250 mm, machined to remove scale and decarburised skin for precision shafting.
Tolerance: hot rolled bars are supplied to EN 10060 or to the GB/T 702 tolerance groups; cold drawn and peeled bars are typically held to h9 to h11 with a surface roughness around Ra 3.2 µm.
Lengths: 3 m to 12 m in fixed or random lengths, with cutting to size on request.
Welding, Machining and Typical Applications
S355 bars weld readily with common arc processes, provided the welding procedure accounts for the carbon equivalent and the section diameter; thicker bars and restrained joints may need preheating, and consumables should be stored dry to keep hydrogen out of the joint. Machining behaviour is typical of a low-carbon structural steel: continuous chips, moderate tool wear and good dimensional stability after machining, although the surface finish is coarser than that of a free-cutting or medium-carbon grade. Applications include anchor bars and holding down bolts, tie rods, bracing members, crane and conveyor components, machined shafts and pins, and structural connections where a higher strength than S235 is needed without moving to an alloy steel.
Frequently Asked Questions
Q: What is the difference between S355JR and S355J2?
The strength requirements are identical and both grades guarantee 27 J impact energy, but they guarantee it at different temperatures. S355JR is tested at +20 °C and S355J2 at −20 °C, and S355J2 also carries tighter phosphorus and sulphur limits. The J2 grade is therefore the correct choice for outdoor structures, cold climate service and components subject to dynamic loading, while JR is adequate for normal temperature, predominantly static duty.
Q: What is the current equivalent of S355J2G3?
S355J2G3 belonged to the earlier EN 10025 edition, where the suffix indicated the delivery condition and the impact test temperature. In the current standard the delivery condition is stated separately, as in S355J2+N for normalised rolling, and the designation itself has become S355J2. The strength and the 27 J at −20 °C impact requirement are unchanged, so the conversion is a change of name rather than of technical requirement.
Q: Is S355 an alloy steel bar?
No. S355JR, S355J0, S355J2 and S355K2 are non-alloy structural steels under EN 10025-2. The strength comes from manganese and from the rolling or heat treatment condition, not from alloying with chromium, nickel or molybdenum. Bars that are genuinely alloy steel, for example chromium-molybdenum grades supplied quenched and tempered for high stress components, are specified under different standards and have a different welding and heat treatment regime.
Q: Can S355 round bars be welded without preheating?
In many cases yes, particularly for small diameters and low restraint joints made with a controlled heat input. The decision should be based on the carbon equivalent, the bar diameter, the joint restraint and the ambient temperature, following a recognised welding procedure such as EN 1011-2. Where the calculation indicates a risk of cold cracking, preheat and interpass temperature control, or a post-weld treatment, become mandatory; the requirement should be established before fabrication rather than on site.
Q: Which grade should be used at low service temperatures?
S355J2 guarantees 27 J at −20 °C and S355K2 guarantees 40 J at the same temperature, so either is suitable for service down to about −20 °C. For colder duty, thermo-mechanically rolled grades in the same strength family are specified with impact testing at −40 °C or −50 °C. The rule is to select from the minimum design metal temperature of the component rather than from the ambient temperature at the fabrication site.
Q: How should an S355 bar order be specified?
State the standard, the full designation including the impact suffix, the delivery condition where relevant, the diameter and its tolerance class, the delivery length and tolerance, the surface condition and the inspection documents required. A mill test certificate to EN 10204 3.1 should give the heat number, chemical analysis including carbon equivalent, tensile results with yield strength, tensile strength and elongation, and the impact energy at the grade test temperature. Where the bar will be machined, the tolerance and surface finish are as important as the grade.